| Material:: | Stainless Steel And Special Alloys | Standard:: | AMS 5604, ASTM A 693, ASME SA 693 |
|---|---|---|---|
| UNS:: | S17400 | Grade:: | 17-7 PH |
| Shape:: | Round,Square,Flat,Angle | Application:: | Construction,Industry,surgical Tools |
| Certification:: | ISO,BV,SGS,Mill Test Certificate | Dimensions:: | 3-400mm |
17-4 PH is een gedeponeerd handelsmerk van AK Steel.
| NS: | S17400 |
| Specificaties: | AMS 5604, ASTM A 693, ASME SA 693 |
| Internationale specificaties: | Euronorm: X5CrNiCuNb16.4 Werstoff# 1.4542 |
De volgende tabel toont de chemische samenstelling van roestvrij staal van klasse 17-4.
| Element | Inhoud (%) |
|---|---|
| IJzer, fe | 73 |
| Chroom, Cr | 15.0 - 17.5 |
| Nikkel, Ni | 3.0 - 5.0 |
| Koper, Cu | 3.0 - 5.0 |
| Mangaan, Mn | 1.0 |
| Silicium, Si | 1.0 |
| Tantaal, Ta | 0,45 |
| Niobium, Nb (Columbium, Cb) | 0,45 |
| Nb + Ta | 0,15 - 0,45 |
| Koolstof, C | 0.070 |
| Fosfor, P | 0.040 |
| Zwavel, S | 0.030 |
De fysische eigenschappen van roestvrij staal van klasse 17-4 worden gegeven in de volgende tabel.
| Eigenschappen | Metriek | Keizerlijk |
|---|---|---|
| Dikte | 7,75 g/cm²3 | 0,280 lb/in³ |
De mechanische eigenschappen van gegloeid roestvrij staal van klasse 17-4 worden weergegeven in de volgende tabel.
| Eigenschappen | Metriek | Keizerlijk |
|---|---|---|
| Afschuifmodulus | 77,4 GPa | 11200 kilo |
| Elasticiteitsmodulus | 190-210 GPa | 27557-30458 ksi |
| Poisson-ratio | 0,27-0,30 | 0,27-0,30 |
| Hardheid, Brinell | 352 | 352 |
| Hardheid, Knoop (geschat op basis van Rockwell C) | 363 | 363 |
| Hardheid, Rockwell C | 36 | 36 |
| Hardheid, Vickers (geschat op basis van Rockwell C) | 349 | 349 |
![]()
![]()